Tenax Epoxart Kit 4:1 — Fast-Cure, Natural-Effect Epoxy for Stone & Granite Reinforcement

SKU: EPOXARTKIT4TO1
No reviews

Price:
Sale price$76.55

Description

When speed matters and preserving the stone's original color is non-negotiable, Tenax Epoxart Kit 4:1 is the professional's choice. Its 7–8 minute gel time and 6–8 hour polish-ready cure (at 77–95°F / 25–35°C) get you back to grinding, polishing, or installing faster — while its natural-effect formulation leaves the stone looking exactly as it should. No darkening, no tinting, no color shift. Combined with good UV stability and superb cold reactivity, this is the go-to epoxy for high-volume fabrication shops and white or color-sensitive materials.

Key Features

  • Fastest cure in the Epoxart line — 7–8 min gel time; polish or cut in 6–8 hrs at 77–95°F (25–35°C)
  • Natural effect — formulated to leave stone color unchanged; the pick for white materials sensitive to halos
  • Thickest consistency of the three — runny-honey body stays on the surface and in the repair; does not migrate into surrounding stone
  • Good UV stability — suitable for outdoor stone surfaces and sun-exposed installations
  • Superb cold reactivity — cures reliably in cold shop or jobsite environments
  • Medium hardness — Shore D 78–80; balanced flexibility to resist re-cracking under load
  • Batch small — 7-min pot life means mix only what you can spread in ~5 min

Cure Times (from Tenax TDS rev 03, 09/2025)

  • Gel time in cup @ 77°F (25°C): 7–8 min
  • Tack-free @ 77°F (25°C): 100–110 min
  • Ready to polish/cut @ 77–95°F (25–35°C): 6–8 hrs
  • Ready to polish/cut @ 59–77°F (15–25°C): 24–48 hrs
  • Minimum cure temp: 59°F (15°C)
  • Service range after cure: -13°F to 140°F (-25°C to +60°C)

Ideal Applications

  • Production environments requiring fast turnaround — get the slab back in the line this shift
  • White and light-colored stone sensitive to halos or resin migration
  • Surface consolidation and facework where body and fill are needed
  • Cold-weather fabrication and outdoor jobsite applications
  • Outdoor stone surfaces, pavers, and cladding exposed to sunlight

Epoxart Kit A+B — Which Ratio Do You Need?

Same proven Tenax epoxy chemistry, three cure profiles. Every kit includes Part A (resin) and Part B (hardener) — always mixed together by weight. All three cure to the same hardness (Shore D 77–80). The difference is cure speed, flow, and sunlight stability.

EPOXART 2:1

The crack repair kit

Very fluid with excellent adhesion. Reach for it on crack repairs, laminated edges, fiberglass netting, and colored materials.

EPOXART 3:1

The penetration kit

Thinnest flow, longest open time, and the best sunlight stability in the line. Reach for it on porous or fractured stone and outdoor work.

EPOXART 4:1 ★ THIS KIT

The speed kit

Accelerated cure — polish or cut in 6–8 hours. The pick for white materials sensitive to halos. Mix small batches: pot life is minutes, not hours.

Spec 2:1 3:1 4:1 ★
Mix ratio (A : B, by weight) 2 : 1 3 : 1 4 : 1
Mixed consistency Thin syrup — very fluid, wets out mesh and laminations Thin syrup — thinnest of the three, deepest soak-in Runny honey — stays where you put it
Working time in the cup — 77°F (25°C) 55–75 min 150–180 min 7–8 minutes
Tack-free — 77°F (25°C) ~240 min 300–360 min 100–110 min
Ready to polish / cut — shop temp 77–95°F (25–35°C) 8-24 hrs 24–48 hrs 6–8 hrs
Ready to polish / cut — cool shop 59–77°F (15–25°C) 48 hrs 48–72 hrs 24–48 hrs
Sunlight stability (3-yr Xenon test, ISO 11341) Medium-good — made for laminated & colored work Good — best of the three Good
Best for Crack repairs, lamination, fiberglass netting, colored materials Porous / fractured stone, outdoor work Production speed, halo-sensitive white materials
Cured hardness (Shore D) 77–80 78–80 78–80
Minimum shop temp to cure 59°F (+15°C) — all kits
Service temp after full cure -13°F to 140°F (-25°C to +60°C) — all kits

Every kit, every time:

  • Mix Part A + Part B by weight, not volume — the ratio is in the kit name.
  • Stone must be completely dry and clean before resining.
  • 4:1 users: mix only what you can apply in about 5 minutes. Pot life is 7–8 minutes at 77°F (25°C).
  • Never use PVC containers; keep resin away from copper and brass.
  • Gloves and safety glasses required. See the SDS before use.
  • Store sealed in original containers at 68–77°F (20–25°C). Do not let the resin freeze. Shelf life 24 months.

Data: Tenax S.p.A. technical data sheets rev 03 (03/09/2025). Laboratory values, indicative — always test on your specific material.

Kit Contents

  • Epoxart A-1006 — 1 kg (Resin, Part A)
  • Epoxart B-BB25 — 0.25 kg (Hardener, Part B)
  • Total kit weight: 1.25 kg
  • Mix ratio: 4 parts resin : 1 part hardener (by weight)

How to Use

  1. Clean and thoroughly dry the stone surface — remove all dust, oils, and debris.
  2. Measure by weight: 4 parts resin (Part A) to 1 part hardener (Part B).
  3. Mix thoroughly using clean corrosion-resistant plastic tools — never PVC, copper, or brass.
  4. Apply wearing safety gloves and glasses. Work fast — 7–8 min pot life.
  5. Reseal containers immediately; never let the resin freeze.

Storage & Shelf Life

  • Store below 35°C (95°F), away from heat, direct sunlight, humidity, and freezing
  • Shelf life: 24 months sealed at 68–77°F (20–25°C)

Not sure which Epoxart ratio is right for your job?

Read our full comparison: Tenax Epoxart 2:1 vs 3:1 vs 4:1 — Which Stone Epoxy Ratio Do You Actually Need?

Choosing the Right Epoxart Kit

  • Epoxart Kit 2:1 — very fluid, high-adhesion; best for lamination, fiberglass netting, and colored materials
  • Epoxart Kit 3:1 — thinnest flow, longest open time; best for porous/fractured stone and outdoor work
  • Epoxart Kit 4:1 (this product) — fastest cure, natural effect; best for production speed and white/color-sensitive stone

Works Well With

Technical data from Tenax S.p.A. technical data sheets rev 03 (03/09/2025). All values are laboratory results and indicative; always test on your specific material.

You may also like

Recently viewed